Inconel 718及其渗铝涂层在Na2SO4 + 5%NaCl混合盐膜下的热腐蚀行为
胡琪, 耿树江, 王金龙, 王福会, 孙清云, 吴勇, 夏思瑶

Hot Corrosion Behavior of Inconel 718 Without and With Aluminide Coating in Air Beneath a Thin Film of Salt Mixture of Na2SO4 + 5%NaCl
HU Qi, GENG Shujiang, WANG Jinlong, WANG Fuhui, SUN Qingyun, WU Yong, XIA Siyao
图2 Inconel 718合金和CVD渗Al涂层在750,850和950℃下Na2SO4 + 5%NaCl混合盐膜下的热腐蚀50 h的质量变化曲线
Fig.2 Mass change curves of Inconel 718 alloy and CVD aluminide coating deposited with Na2SO4 + 5%NaCl during hot corrosion for 50 h in air at 750, 850 and 950℃