单相流冲刷条件下一种低合金高强钢的腐蚀行为研究
傅江悦, 郭建喜, 杨延格, 冷哲, 王文

Erosion-corrosion Behavior of a High Strength Low Alloy Steel in Flowing 3.5%NaCl Solution
FU Jiangyue, GUO Jianxi, YANG Yange, LENG Zhe, WANG Wen
表2 文献中关于腐蚀产物的Raman位移[47~50]
Table 2 Raman shifts of various typical corrosion products in literatures[47~50]
PhaseRaman shift / cm-1
Lepidocrocite (γ-FeOOH)166, 217, (248-257), 310, 350, (376-393), (478-530), (526-530), (650-655), 713, (1300-1310)
Goethite (α-FeOOH)203, (241-250), (298-307), (385-399), (414-415), (474-483), (549-554), 684, 1002, 1113, 1304
Akaganeite (β-FeOOH)139, (308-314), 331, (385-390), (415-420), (497-499), (526-541), (720-745)
Magnetite (Fe3O4)(298-306), (535-550), 616, (663-670)
Maghemite (γ-Fe2O3)(339-386), (461-512), (500-506), (671-717), (700-720), (1400-1440)