单相流冲刷条件下一种低合金高强钢的腐蚀行为研究
傅江悦, 郭建喜, 杨延格, 冷哲, 王文

Erosion-corrosion Behavior of a High Strength Low Alloy Steel in Flowing 3.5%NaCl Solution
FU Jiangyue, GUO Jianxi, YANG Yange, LENG Zhe, WANG Wen
图12 HSLA钢在静态浸泡不同时间后的宏观形貌
Fig.12 Macroscopic morphologies of HSLA steel after static immersion for 2 h (a), 12 h (b), 72 h (c), 216 h (d), 288 h (e),384 h (f) and 480 h (g)