镁合金腐蚀测试与分析研究进展
|
黄居峰, 宋光铃
|
Research Progress on Corrosion Testing and Analysis of Mg-alloys
|
HUANG Jufeng, SONG Guangling
|
|
表1 不同镁合金腐蚀速率的比较
|
Table 1 Comparison of corrosion rates of various Mg-alloys
|
|
Material | Solution | Time | Method | Corrosion rate / mm·a-1 | Reference |
---|
Mg5Y | 3.5%NaCl | 300 h | Hydrogen collection | 4.1 | [22] | Mg5Y | 3.5%NaCl | 400 s | Tafel extrapolation | 0.4 | [22] | Mg5Li1Al | 3.5%NaCl | 14 d | Mass loss | 38 | [23] | Mg5Li1Al | 3.5%NaCl | 20 m | Tafel extrapolation | 22 | [23] | AZ91 | 3.5%NaCl | 24 h | Mass loss | 1.6 | [24] | AZ91 | 3.5%NaCl | 15 m | Tafel extrapolation | 1.3 | [24] | Mg0.06Cu | Hanks solution | 7 d | Mass loss | 30 | [25] | Mg0.06Cu | Hanks solution | 30 m | Tafel extrapolation | 0.12 | [25] | Mg0.14In | 0.1 mol/L NaCl | 1 d | Mass loss | 7 | [26] | Mg0.14In | 0.1 mol/L NaCl | 10 m | Tafel extrapolation | 0.6 | [26] | Pure Mg | 0.1 mol/L NaCl | 1 d | Mass loss | 0.8 | [26] | Pure Mg | 0.1 mol/L NaCl | 10 m | Tafel extrapolation | 0.3 | [26] | Pure Mg | NaCl+ZnCl2 | 41.3 h | Hydrogen collection | 12 | [27] | Pure Mg | NaCl+ZnCl2 | 41.3 h | Mass loss | 14 | [27] | Pure Mg | 0.4 mol/L Na2SO4 | 7 d | Hydrogen collection | 0.5 | [28] | Pure Mg | 0.4 mol/L Na2SO4 | 7 d | AC impedance | 0.2 | [28] | Pure Mg | 0.4 mol/L (NH4)2SO4 | 7 d | Hydrogen collection | 16 | [28] | Pure Mg | 0.4 mol/L (NH4)2SO4 | 7 d | AC impedance | 12 | [28] |
|
|
|