3Cr合金钢在尿素辅助稠油蒸汽吞吐环境中的初期腐蚀行为
张运军, 蒋有伟, 张忠义, 吕乃欣, 陈君伟, 连国锋

Initial Corrosion Behavior of 3Cr Alloy Steel in Urea Assisted Heavy Oil Steam Huff and Puff Environments
ZHANG Yunjun, JIANG Youwei, ZHANG Zhongyi, LV Naixin, CHEN Junwei, LIAN Guofeng
图10 3Cr合金钢在50和80℃下不同比例原油与30%浓度尿素溶液的混合液中腐蚀后的宏观形貌
Fig.10 Macro appearances of 3Cr alloy steel after corrosion at 50oC (a, b) and 80oC (c, d) in mixed solutions with the different proportions of crude oil and 30% urea solution: (a, c) 9∶1, (b, d) 8∶2