形变强化和逆相变细晶强化对Fe-18Cr-8Ni钢耐腐蚀性能的影响
王智慧, 吴雷, 姜懿珊, 张弦, 万响亮, 李光强, 吴开明

Effect of Deformation Strengthening and Phase Reversion Grain Refinement Strengthening on Corrosion Resistance of Fe-18Cr-8Ni Steel
WANG Zhihui, WU Lei, JIANG Yishan, ZHANG Xian, WAN Xiangliang, LI Guangqiang, WU Kaiming
表1 3种钢试样在3.5%NaCl溶液中的点蚀电位、腐蚀电位和腐蚀电流密度
Table 1 Pitting potential (Epit), corrosion potensial (Ecorr) and corrosion current density (Icorr) of three steels in 3.5%NaCl solution
Steel sampleEpit / VEcorr / V vs SCEIcorr / A·cm-2
Original0.41-0.381.02 × 10-14
CR0.48-0.982.47 × 10-11
UFG/FG0.75-1.125.09 × 10-10