某燃气轮机燃烧室合金高温蒸汽氧化行为研究 |
梁志远, 张超, 曲劲宇, 何建元, 郭亭山, 徐一鸣 |
Oxidation Behavior in Air-steam Mixed Atmosphere at 1000oC of Four Typical High-temperature Alloys for Gas Turbine |
LIANG Zhiyuan, ZHANG Chao, QU Jinyu, HE Jianyuan, GUO Tingshan, XU Yiming |
图10 K447A合金氧化100和300 h后断面形貌与EDS元素分布分析 |
Fig.10 Cross-sectional morphologies (a, c) and EDS element distributions (b, d) of K447A superalloy oxidized for 100 h (a, b) and 300 h (c, d) |
![]() |