某燃气轮机燃烧室合金高温蒸汽氧化行为研究
梁志远, 张超, 曲劲宇, 何建元, 郭亭山, 徐一鸣

Oxidation Behavior in Air-steam Mixed Atmosphere at 1000oC of Four Typical High-temperature Alloys for Gas Turbine
LIANG Zhiyuan, ZHANG Chao, QU Jinyu, HE Jianyuan, GUO Tingshan, XU Yiming
图4 合金DD5氧化100、200和300 h后表面的SEM形貌
Fig.4 Low (a-c) and high (d) magnification SEM images of DD5 supper alloy after oxidation for 100 h (a), 200 h (b) and 300 h (c, d)