含双腐蚀缺陷管道的氢浓度分布模拟
郭诗雯, 吴浩志, 董绍华, 陈林, 程玉峰

Simulation of Hydrogen Distribution in Pipeline with Double Corrosion Defects
GUO Shiwen, WU Haozhi, DONG Shaohua, CHEN Lin, CHENG Frank
表2 不同缺陷长度下,不同间距的双缺陷处氢浓度最大值
Table 2 Maximum hydrogen concentrations at double defects with different lengths and different spacing under different tensile strains (mol/m3)
Tensile strain/%Defect length/mm
81012
0101010
0.110.1410.0910.06
0.210.7310.5510.43
0.511.2310.9810.79*
0.611.3211.08*10.95*
111.88*11.68*11.46*
213.21*13.01*12.53*
314.01*13.91*13.36*