微合金化对高锰奥氏体钢在酸性盐雾环境下的耐蚀性能影响研究
常雪婷, 宋嘉琪, 王冰, 王东胜, 陈文聪, 王海丰

Effect of Micro-alloying with Cr, N and Al on Corrosion Resistance of High Manganese Austenitic Steel in Acidic Salt Spray Environment
CHANG Xueting, SONG Jiaqi, WANG Bing, WANG Dongsheng, CHEN Wencong, WANG Haifeng
表5 两种高锰钢腐蚀动力学拟合结果
Table 5 Fitting results of corrosion kinetic curves of two experimental steels
SampleWR2n
WH-HMSW = 4.44202 × 10-4t0.96180.987270.9618
PT-HMSW = 8.74985 × 10-4t0.677590.992820.6776