碳钢和高强钢在南海大气环境中的初期腐蚀行为研究 |
| 王靖羽, 周学杰, 王洪伦, 吴军, 陈昊, 郑鹏华 |
|
Initial Corrosion Behavior of Carbon Steel and High Strength Steel in South China Sea Atmosphere |
| WANG Jingyu, ZHOU Xuejie, WANG Honglun, WU Jun, CHEN Hao, ZHENG Penghua |
| 图7 4种钢材在南海海洋大气环境中腐蚀试验0.5和1 a的EIS谱 |
| Fig.7 Nyquist (a1, a2), impedance module (b1, b2) and phase angle (c1, c2) plots of four kinds of steels after 0.5 a (a1-c1) and 1 a (a2-c2) corrosion in the marine atmosphere of the South China Sea |
|