碳钢和高强钢在南海大气环境中的初期腐蚀行为研究 |
王靖羽, 周学杰, 王洪伦, 吴军, 陈昊, 郑鹏华 |
Initial Corrosion Behavior of Carbon Steel and High Strength Steel in South China Sea Atmosphere |
WANG Jingyu, ZHOU Xuejie, WANG Honglun, WU Jun, CHEN Hao, ZHENG Penghua |
图3 4种钢材0.5和1a后除锈前和除锈后的微观腐蚀形貌 |
Fig.3 Corrosion morphologies of Q235B (a1-a4), Q350EWR1 (b1-b4), Q355 (c1-c4) and Q345NQR2 (d1-d4) steels exposed to atmospheric environment of the South China Sea for 0.5 a (a1-d1, a2-d2) and 1 a (a3-d3, a4-d4) before (a1-d1, a3-d3)and after (a2-d2, a4-d4) removing rust |
![]() |