超临界水环境中三种Ni-Cr涂层氧化特性研究
袁小虎, 李定骏, 王天剑, 郭显平, 张乃强, 朱忠亮

Oxidation Behavior of Three Different Ni-Cr Coatings in 630oC/25 MPa Supercritical Water
YUAN Xiaohu, LI Dingjun, WANG Tianjian, GUO Xianping, ZHANG Naiqiang, ZHU Zhongliang
图11 FB2合金及不同Ni-Cr涂层在630℃超临界水环境中氧化3000 h后的横截面形貌及元素分布图
Fig.11 Cross-sectional morphologies (a1-d1) and corresponding elemental depth profiles (a2-d2) of FB2 alloy (a1, a2) and thermally sprayed Ni-Cr coatings untreated (b1, b2) and treated by shot peening (c1, c2) and grinding (d1, d2) after exposure in SCW at 630oC for 3000 h