超临界水环境中三种Ni-Cr涂层氧化特性研究 |
袁小虎, 李定骏, 王天剑, 郭显平, 张乃强, 朱忠亮 |
Oxidation Behavior of Three Different Ni-Cr Coatings in 630oC/25 MPa Supercritical Water |
YUAN Xiaohu, LI Dingjun, WANG Tianjian, GUO Xianping, ZHANG Naiqiang, ZHU Zhongliang |
图6 FB2基材在630℃/25 MPa超临界水中氧化3000 h后的表面形貌 |
Fig.6 Surface morphologies of the spallation zones of the oxide scale formed on FB2 steel exposed in 630oC/25 MPa SCW for 3000 h: (a) low-magnification view, (b) high-magnification view of location 1, (c) low-magnification view, (d) high-magnification view of location 2, (e) high-magnification view of location 3, (f) high-magnification view of location 4 |
![]() |