超临界水环境中三种Ni-Cr涂层氧化特性研究 |
袁小虎, 李定骏, 王天剑, 郭显平, 张乃强, 朱忠亮 |
Oxidation Behavior of Three Different Ni-Cr Coatings in 630oC/25 MPa Supercritical Water |
YUAN Xiaohu, LI Dingjun, WANG Tianjian, GUO Xianping, ZHANG Naiqiang, ZHU Zhongliang |
图5 FB2基材以及喷涂态、喷丸态和磨削态Ni-Cr涂层在630℃/25 MPa超临界水中氧化1000 h后的表面形貌 |
Fig.5 Surface morphologies of FB2 steel (a, b) and Ni-Cr thermally sprayed coatings untreated (c, d) and treated by shot peening (e, f) and grinding (g, h) after exposure in 630oC/25 MPa SCW for 1000 h |
![]() |