超临界水环境中三种Ni-Cr涂层氧化特性研究
袁小虎, 李定骏, 王天剑, 郭显平, 张乃强, 朱忠亮

Oxidation Behavior of Three Different Ni-Cr Coatings in 630oC/25 MPa Supercritical Water
YUAN Xiaohu, LI Dingjun, WANG Tianjian, GUO Xianping, ZHANG Naiqiang, ZHU Zhongliang
图3 630℃/25 MPa超临界水中FB2基材、喷涂态、喷丸态以及磨削态NiCr涂层不同氧化时间后的表面形貌