Ni含量对Co-Al-W合金热腐蚀行为的影响 |
| 王华, 王英杰, 刘恩泽 |
|
Hot Corrosion Behavior of New Type Co-Al-W Superalloys with Different Ni Contents |
| WANG Hua, WANG Yingjie, LIU Enze |
| 图6 合金A在900 °C下75% Na2SO4+25% NaCl的混合熔盐中热腐蚀32 h后的SEM形貌和EDS谱 |
| Fig.6 SEM morphology of the alloy A after hot corrosion in 75% Na2SO4+25% NaCl at 900 °C for 32 h (a), and EDS mappings of Al (b), Co (c), Ni (d), O (e), S (f) and W (g) |
|