Ni含量对Co-Al-W合金热腐蚀行为的影响 |
王华, 王英杰, 刘恩泽 |
Hot Corrosion Behavior of New Type Co-Al-W Superalloys with Different Ni Contents |
WANG Hua, WANG Yingjie, LIU Enze |
图5 3种合金在900 °C下Na2SO4和NaCl的熔盐混合物中热腐蚀32 h后的横截面SEM显微照片 |
Fig.5 Cross-sectional micrographs of alloys A (a), B (b) and C (c) after hot corrosion in Na2SO4 and NaCl molten salt at 900 °C for 32 h |
![]() |