Ni含量对Co-Al-W合金热腐蚀行为的影响 |
王华, 王英杰, 刘恩泽 |
Hot Corrosion Behavior of New Type Co-Al-W Superalloys with Different Ni Contents |
WANG Hua, WANG Yingjie, LIU Enze |
图4 合金在900 °C下75% Na2SO4+25% NaCl熔盐中腐蚀不同时间后的SEM表面形态 |
Fig.4 SEM surface morphologies of three alloys A (a-d), B (e-h) and C (i-l) after hot corrosion in 75% Na2SO4+25% NaCl molten salt at 900 °C for 2 h (a, b, e, f, i, j) and 32 h (c, d, g, h, k, l) |
![]() |