Ni含量对Co-Al-W合金热腐蚀行为的影响 |
王华, 王英杰, 刘恩泽 |
Hot Corrosion Behavior of New Type Co-Al-W Superalloys with Different Ni Contents |
WANG Hua, WANG Yingjie, LIU Enze |
图3 在900 ℃下75% Na2SO4+25% NaCl熔盐中热腐蚀2、16、32 h后腐蚀产物的XRD图谱 |
Fig.3 XRD patterns of corrosion products formed on three Co-Al-W-xNi superalloys after hot corrosion at 900 ℃ in 75% Na2SO4+25% NaCl molten salt for 2 (a), 16 (b) and 32 h (c) |
![]() |