CMAS熔体在不同热障涂层用材料表面的铺展和腐蚀行为 |
| 曲卫卫, 陈泽浩, 裴延玲, 李树索, 王福会 |
|
Spreading and Corrosion Behavior of CMAS Melt on Different Materials for Thermal Barrier Coating |
| QU Weiwei, CHEN Zehao, PEI Yanling, LI Shusuo, WANG Fuhui |
| 图 4 不同陶瓷样品1250 ℃处理16 h后反应层剖面形貌 |
| Fig.4 Cross-sectional morphologies of the reaction layers of different ceramic samples with CMAS deposit after treatment at 1250 ℃ for 16 h: (a) YSZ, (b) YSHf, (c) Al2O3, (d) LCO, (e) GZO, (f) Y2O3 |
|