CMAS熔体在不同热障涂层用材料表面的铺展和腐蚀行为 |
| 曲卫卫, 陈泽浩, 裴延玲, 李树索, 王福会 |
|
Spreading and Corrosion Behavior of CMAS Melt on Different Materials for Thermal Barrier Coating |
| QU Weiwei, CHEN Zehao, PEI Yanling, LI Shusuo, WANG Fuhui |
| 图3 陶瓷片经CMAS在1250 ℃处理16 h后的XRD谱 |
| Fig.3 XRD patterns of different ceramics with CMAS deposit after treatment at 1250 ℃ for 16 h |
|