表3 不同种类超滑涂层的耐蚀性能对比
|
Table 3 Comparison of corrosion resistance of different kinds of slippery/superhydrophobic coatings
|
|
| Coating | Coating category | Corrosion test conditions | Result comparison |Z|0.01 Hz / Ω·cm2 |
|---|
| SiO2-25 | slippery coating | 3.5%NaCl solution immersion | 0 d | 20 d | | 3.22×1011 | 6.62×109 | | KCC-1/PVDF[12] | Superhydrophobic coating | 1 d | 14 d | | 4.9×108 | 1.13×108 | | KCC-1/PVDF-SLIPS[12] | slippery coating | 1 d | 14 d | | 1.31×1010 | 1.02×109 | | LDH-PFDS[24] | Superhydrophobic coating | 7 d | | 8.36×106 | | LDH-PFDS-SLIPS[24] | slippery coating | 7 d | | 1.34×107 | | PDMS-SiO2/PANI[25] | Superhydrophobic coating | 1 h | 8 d | | ~109 | ~108 | | TMES-modifified SiO2 matrix coating[26] | Superhydrophobic coating | 0 d | 5 d |
|
|
|