四元MAX相(Cr2/3Ti1/3)3AlC2 在高温空气以及水蒸气气氛中的氧化行为研究 |
||||||||||||||||||||
任岩, 张鑫涛, 盖欣, 徐敬军, 张伟, 陈勇, 李美栓 | ||||||||||||||||||||
High Temperature Oxidation Behavior of Quaternary (Cr2/3Ti1/3)3AlC2 MAX Ceramic in Air and Steam |
||||||||||||||||||||
REN Yan, ZHANG Xintao, GAI Xin, XU Jingjun, ZHANG Wei, CHEN Yong, LI Meishuan | ||||||||||||||||||||
表1 水蒸气中氧化后表面能谱分析结果 (atomic fraction / %) |
||||||||||||||||||||
Table 1 EDS results of the surfaces of (Cr2/3Ti1/3)3AlC2 samples after oxidation in water vapor |
||||||||||||||||||||
|
||||||||||||||||||||