四元MAX相(Cr2/3Ti1/3)3AlC2 在高温空气以及水蒸气气氛中的氧化行为研究 |
任岩, 张鑫涛, 盖欣, 徐敬军, 张伟, 陈勇, 李美栓 |
High Temperature Oxidation Behavior of Quaternary (Cr2/3Ti1/3)3AlC2 MAX Ceramic in Air and Steam |
REN Yan, ZHANG Xintao, GAI Xin, XU Jingjun, ZHANG Wei, CHEN Yong, LI Meishuan |
图10 (Cr2/3Ti1/3)3AlC2在1000和1200 ℃下水蒸气中氧化后的表面X射线衍射谱图 |
Fig.10 XRD patterns of the surfaces of (Cr2/3Ti1/3)3AlC2 after oxidation at 1000 and 1200 ℃ in water vapor |
![]() |