四元MAX相(Cr2/3Ti1/3)3AlC2 在高温空气以及水蒸气气氛中的氧化行为研究 |
任岩, 张鑫涛, 盖欣, 徐敬军, 张伟, 陈勇, 李美栓 |
High Temperature Oxidation Behavior of Quaternary (Cr2/3Ti1/3)3AlC2 MAX Ceramic in Air and Steam |
REN Yan, ZHANG Xintao, GAI Xin, XU Jingjun, ZHANG Wei, CHEN Yong, LI Meishuan |
图5 (Cr2/3Ti1/3)3AlC2在800 ℃下空气中氧化后的截面微观形貌及元素分布 |
Fig.5 Cross-sectional morphology (a) and corresponding element profiles (b) of (Cr2/3Ti1/3)3AlC2 after oxidation at 800 ℃ in air |
![]() |