铅基堆结构材料液态金属腐蚀行为的研究进展 |
| 张心怡, 李聪, 汪禹熙, 黄美, 朱卉平, 刘芳, 刘洋, 牛风雷 |
|
Research Progress on Liquid Metal Corrosion Behavior of Structural Steels for Lead Fast Reactor |
| ZHANG Xinyi, LI Cong, WANG Yuxi, HUANG Mei, ZHU Huiping, LIU Fang, LIU Yang, NIU Fenglei |
| 图3 流速5 m/s的铅铋垂直冲刷1000 h后T91钢截面铅铋侵蚀形貌,Kernel局部平均取向差及反极图+花样质量叠加图[ |
| Fig.3 BSE image of a typical LBE penetration path on the cross section of T91 after exposure to perpendicular LBE flow at a fluid rate of 5 m/s for 1000 h (a), Kernel average misorientation map (b) and inverse pole figure+image quality map corresponding to the area bordered with yellow line in Fig.3a (c)[ |
|