铅基堆结构材料液态金属腐蚀行为的研究进展 |
张心怡, 李聪, 汪禹熙, 黄美, 朱卉平, 刘芳, 刘洋, 牛风雷 |
Research Progress on Liquid Metal Corrosion Behavior of Structural Steels for Lead Fast Reactor |
ZHANG Xinyi, LI Cong, WANG Yuxi, HUANG Mei, ZHU Huiping, LIU Fang, LIU Yang, NIU Fenglei |
图2 800 ℃铅铋腐蚀后FeCrAl合金样品截面同步X射线劳厄衍射平均峰宽分布图及对应于图2a中不同深度各点的局部劳厄衍射峰[ |
Fig.2 Distribution of average peak width given by synchronous X-ray Laue diffraction on the cross section of FeCrAl alloy after liquid LBE corrosion at 800 ℃ (a) and local Laue diffraction peaks at different depths corresponding to the points marked in Fig.2a (b-d)[ |
![]() |