超高性能海水海砂混凝土的硫酸盐腐蚀破坏机理研究 |
李田雨, 王维康, 李扬涛, 包腾飞, 赵梦凡, 沈欣欣, 倪磊, 马庆磊, 田惠文 |
Corrosion Failure Mechanism of Ultra-high-performance Concretes Prepared with Sea Water and Sea Sand in an Artificial Sea Water Containing Sulfate |
LI Tianyu, WANG Weikang, LI Yangtao, BAO Tengfei, ZHAO Mengfan, SHEN Xinxin, NI Lei, MA Qinglei, TIAN Huiwen |
图6 硫酸盐腐蚀6个月后SSUHPC的内部 |
Fig.6 Inner area (a, d-f) and EDS mapping (b, c) of SSUHPC after sulfate corrosion for 6 months |
![]() |