水溶性缓蚀剂对建筑管道用Q235钢腐蚀行为的影响 |
何静, 于航, 傅梓瑛, 岳鹏辉 |
Effect of Water-soluble Corrosion Inhibitor on Corrosion Behavior of Q235 Pipeline Steel for Construction |
HE Jing, YU Hang, FU Ziying, YUE Penghui |
图10 浸泡168 h后沉积物覆盖下Q235钢的显微腐蚀形貌 |
Fig.10 Surface morphology of corrosion scales of sediment-covered Q235 steel after 168 h immersion: (a) without inhibitor, (b) 8 mg/L, (c) 15 mg/L, (d) 25 mg/L |
![]() |