缝隙腐蚀内部微区离子浓度监测的研究进展
白一涵, 张航, 朱泽洁, 王疆瑛, 曹发和

Research Progress of Monitoring Ion Concentration Variation of Micro-areas in Corrosion Crevice Interior
BAI Yihan, ZHANG Hang, ZHU Zejie, WANG Jiangying, CAO Fahe
图12 201不锈钢在1 mol/L NaCl (pH=4.00) 溶液中,缝隙内部不同位置处Cl-浓度随时间的演化图
Fig.12 Evolution of Cl- concentration of 201 stainless steel in 1 mol/L NaCl (pH=4.00) solution at different positions inside the crevice with time