缝隙腐蚀内部微区离子浓度监测的研究进展 |
| 白一涵, 张航, 朱泽洁, 王疆瑛, 曹发和 |
|
Research Progress of Monitoring Ion Concentration Variation of Micro-areas in Corrosion Crevice Interior |
| BAI Yihan, ZHANG Hang, ZHU Zejie, WANG Jiangying, CAO Fahe |
| 图11 201不锈钢在1 mol/L NaCl溶液 (pH=4.00) 中,不同缝隙宽度下缝隙内底部pH随时间演化图 |
| Fig.11 Evolution of the pH value of 201 stainless steel in 1 mol/L NaCl solution (pH=4.00) at the bottom of the crevice with different crevice widths with time |
|