缝隙腐蚀内部微区离子浓度监测的研究进展
白一涵, 张航, 朱泽洁, 王疆瑛, 曹发和

Research Progress of Monitoring Ion Concentration Variation of Micro-areas in Corrosion Crevice Interior
BAI Yihan, ZHANG Hang, ZHU Zejie, WANG Jiangying, CAO Fahe
图8 304不锈钢在不同位置坐标处的pH随时间演化曲线[41]
Fig.8 Comparison of the predicted pH profile change over time for 304 stainless steel at various sites: (a) (0,7), (b) (0,4), (c) (0,0.5) using the current model and experiment[41]