5083-H111铝合金在模拟动态海水环境中的局部腐蚀机制
邓成满, 刘喆, 夏大海, 胡文彬

Localized Corrosion Mechanism of 5083-H111 Al Alloy in Simulated Dynamic Seawater Zone
DENG Chengman, LIU Zhe, XIA Da-Hai, HU Wenbin
图8 5083-H111铝合金在模拟动态海水环境中暴露56 d后表面生成的腐蚀产物的XPS结果
Fig.8 XPS results of corrosion products generated on the surface of 5083-H111 Al alloy after exposed to a simulated dynamic seawater zone for 56 d: (a) Al 2p, (b) O 1s