Q235钢在海南濒海同区域户外暴晒环境和棚下环境的腐蚀行为
|
王洪伦, 杨华, 蔡辉, 李博文
|
Corrosion Behavior of Q235 Steel by Outdoor Exposure and under Shelter in Atmosphere of Hainan Coastal
|
WANG Honglun, YANG Hua, CAI Hui, LI Bowen
|
|
表1 Q235钢各实验组平均失重及腐蚀深度
|
Table 1 Average masslessness and corrosion depth of Q235 steel test groups
|
|
Sample Number | Environment Circle | Average masslessness mg | Corrosion depth D / μm |
---|
311 | Outdoors/Circle 1 | 3.513±0.359 | 18.766±1.920 | 312 | Outdoors/Circle 2 | 6.478±0.233 | 34.601±1.244 | 313 | Outdoors/Circle 3 | 11.425±0.109 | 61.022±0.581 | 314 | Outdoors/Circle 4 | 19.887±0.223 | 106.209±1.193 | 321 | Shed/Circle 1 | 2.481±0.268 | 13.253±1.433 | 322 | Shed/Circle 2 | 4.129±0.085 | 22.052±0.452 | 323 | Shed/Circle 3 | 5.265±0.277 | 28.123±1.478 | 324 | Shed/Circle 4 | 11.163±0.57 | 59.626±3.043 |
|
|
|