两种热处理工艺对3Cr钢腐蚀行为影响及机理研究 |
| 夏晓健, 万芯媛, 陈云翔, 韩纪层, 陈奕扬, 严康骅, 林德源, 陈天鹏, 左晓梅, 孙宝壮, 程学群 |
|
Effect of Heat Treatments on Corrosion Behavior of 3Cr Low Carbon Steel |
| XIA Xiaojian, WAN Xinyuan, CHEN Yunxiang, HAN Jiceng, CHEN Yiyang, YAN Kanghua, LIN Deyuan, CHEN Tianpeng, ZUO Xiaomei, SUN Baozhuang, CHENG Xuequn |
| 图10 正火/退火偶接试样在浸泡30 min前后样品表面SKP电位分布 |
| Fig.10 SKP potential distribution of the normalized/annealed coupled sample before (a) and after (b) immersion for 30 min |
|