两种热处理工艺对3Cr钢腐蚀行为影响及机理研究 |
夏晓健, 万芯媛, 陈云翔, 韩纪层, 陈奕扬, 严康骅, 林德源, 陈天鹏, 左晓梅, 孙宝壮, 程学群 |
Effect of Heat Treatments on Corrosion Behavior of 3Cr Low Carbon Steel |
XIA Xiaojian, WAN Xinyuan, CHEN Yunxiang, HAN Jiceng, CHEN Yiyang, YAN Kanghua, LIN Deyuan, CHEN Tianpeng, ZUO Xiaomei, SUN Baozhuang, CHENG Xuequn |
图7 退火试样及正火试样在0.5%NaCl (pH 3) 溶液中浸泡不同时间后的电化学阻抗谱 |
Fig.7 Nyquist (a, d), impedance module (b, e) and phase angle (c, f) plots of annealed (a-c) and normalized (d-f) samples after soaking in 0.5%NaCl (pH 3) solution for different time |
![]() |