两种热处理工艺对3Cr钢腐蚀行为影响及机理研究 |
| 夏晓健, 万芯媛, 陈云翔, 韩纪层, 陈奕扬, 严康骅, 林德源, 陈天鹏, 左晓梅, 孙宝壮, 程学群 |
|
Effect of Heat Treatments on Corrosion Behavior of 3Cr Low Carbon Steel |
| XIA Xiaojian, WAN Xinyuan, CHEN Yunxiang, HAN Jiceng, CHEN Yiyang, YAN Kanghua, LIN Deyuan, CHEN Tianpeng, ZUO Xiaomei, SUN Baozhuang, CHENG Xuequn |
| 图6 不同热处理条件下3Cr钢浸泡20 d后去除腐蚀产物的微观形貌和3D形貌 |
| Fig.6 Microstructures (a, c) and 3D profile (b, d) of corrosion products removed from 3Cr steel after immersion for 20 d under annealed (a, b) and normalized (c, d) conditions |
|