两种热处理工艺对3Cr钢腐蚀行为影响及机理研究 |
夏晓健, 万芯媛, 陈云翔, 韩纪层, 陈奕扬, 严康骅, 林德源, 陈天鹏, 左晓梅, 孙宝壮, 程学群 |
Effect of Heat Treatments on Corrosion Behavior of 3Cr Low Carbon Steel |
XIA Xiaojian, WAN Xinyuan, CHEN Yunxiang, HAN Jiceng, CHEN Yiyang, YAN Kanghua, LIN Deyuan, CHEN Tianpeng, ZUO Xiaomei, SUN Baozhuang, CHENG Xuequn |
图5 不同热处理条件下3Cr钢试样浸泡2和20 d后的表面腐蚀微观形貌 |
Fig.5 Surface corrosion micro-morphologies of 3Cr steel samples after immersion for 2 d (a, c) and 20 d (b, d) under annealed (a, b) and normalized (c, d) conditions |
![]() |