表1 大气曝露试验试样投样点及其特征环境
|
Table 1 Sampling sites and environmental characteristics of the atmospheric exposure test
|
|
City | Substation | Environment | City | Substation | Environment |
---|
Anqing | H1 | Industrial pollution | Fuyang | K1 | Village | | H4 | Village | | K3 | City | H9 | City | K4 | Village | H12 | Village | K8 | Vity | H13 | Village | T14 | Village | Chizhou | R1 | Industrial pollution | Maanshan | E2 | Industrial pollution | | R5 | City | | E3 | City | R6 | City | E6 | Village | R7 | Village | E7 | Industrial pollution | T25 | Village | E8 | Industrial pollution | Huainan | D1 | Village | Tongling | G2 | Industrial pollution | | D4 | City | | G3 | Industrial pollution | D6 | City | G4 | Industrial pollution | D7 | Village | G7 | Industrial pollution | T28 | Village | T2 | Village |
|
|
|