晶粒尺寸对304L奥氏体不锈钢氢脆的影响 |
王艳飞, 李耀州, 黄玉婷, 谢宏琳, 吴炜杰 |
Effect of Grain Size on Hydrogen Embrittlement of 304L Austenitic Stainless Steel |
WANG Yanfei, LI Yaozhou, HUANG Yuting, XIE Honglin, WU Weijie |
图5 充氢试样断口心部形貌 |
Fig.5 Fracture morphologies of center regions of hydrogen-charged specimens: (a) in situ hydrogen-charged and (b) hydrogen pre-charged AT700-5 specimen, (c) in situ hydrogen-charged, (d) hydrogen pre-charged AT800-20 specimen, (e) in situ hydrogen-charged, (f) hydrogen pre-charged AT1050-20 specimen |
![]() |