晶粒尺寸对304L奥氏体不锈钢氢脆的影响 |
王艳飞, 李耀州, 黄玉婷, 谢宏琳, 吴炜杰 |
Effect of Grain Size on Hydrogen Embrittlement of 304L Austenitic Stainless Steel |
WANG Yanfei, LI Yaozhou, HUANG Yuting, XIE Honglin, WU Weijie |
图4 未充氢试样的断口心部和边缘区域形貌 |
Fig.4 Fracture morphologies of uncharged specimens including both their center regions (a, c, e) and edge regions (b, d, f): (a, b) AT700-5 specimen, (c, d) AT800-20 specimen, (e, f) AT1050-20 specimen |
![]() |