表2 Ni基合金/YSZ涂层1.3 a后的寿命预测结果[39]
Table 2 Life prediction results for Ni-based alloy/YSZ coating after 1.3 a[39]
MatericalPositionTemperature / ℃CoatingCorrosion environmentLife time of coatings / a
GasSteamCorrosivityEffect of Soot BlowerPosition affected by SBPosition not affected by SB
310HcbN2ry SH steam outlet488450YSZ/625StrongWeak>3≥1.5
YSZ/NiCrBSi>3≥1.5
Cr3C2·NiCr<0.3<0.3
Alloy625Tertiary SH steam outlet510500YSZ/625WeakMiddle>3-
YSZ/NiCrBSi>3-
Tertiary SH steam inlet621445YSZ/625StrongStrong>3≥1.5
YSZ/NiCrBSi>3≥1.5