表1 实际垃圾焚烧厂中水冷壁管使用7 a后的腐蚀数据[21]
Table 1 Corrosion data (unit/mm) of water-cooled wall pipes in actual waste incineration plants after 7 a of use[21](mm)
Tube No.MethodPowderSubstrateBefore1 a7 a
1Detonation50Ni-50Cr6.36.856.836.83
250Ni-50Cr+Cr6.46.916.866.83
3Detonation+Are50Ni-50Cr+Al6.57.547.386.99
4DetonationCoCrAlY6.36.656.616.53
5Plasma50Ni-50Cr6.57.727.147.00
6HVOF50Ni-50Cr6.26.646.556.53
780Ni-20Cr6.67.177.026.98
8C-Steel-6.4-6.135.66