超级奥氏体不锈钢的热腐蚀行为及机理研究 |
韩瑞珠, 贾建文, 李阳, 张威, 徐芳泓, 侯利锋, 卫英慧 |
Corrosion Behavior of Three Super Austenitic Stainless Steels in a Molten Salts Mixture at 650-750 ℃ |
HAN Ruizhu, JIA Jianwen, LI Yang, ZHANG Wei, XU Fanghong, HOU Lifeng, WEI Yinghui |
图2 3种不锈钢在不同温度下腐蚀50 h前后的XRD图 |
Fig.2 XRD patterns of 317L (a), 904L (b) and 254SMo (c) stainless steels before and after hot corrosion for 50 h at different temperatures |
![]() |