DZ40M和K452高温合金在NaCl熔盐中的循环热腐蚀行为研究 |
申聚宝, 崔宇, 刘莉, 刘叡, 孟凡帝, 王福会 |
Cyclic Hot Corrosion Behavior of DZ40M and K452 Superalloys Beneath Molten Deposit NaCl |
SHEN Jubao, CUI Yu, LIU Li, LIU Rui, MENG Fandi, WANG Fuhui |
图8 K452合金经不同周次循环热腐蚀后的表面形貌及能谱分析结果 |
Fig.8 Surface morphologies and EDS analysis results of K452 alloy after cyclic hot corrosion for 1 cycle (a), 2 cycles (b), and 15 cycles (c) |
![]() |