DZ40M和K452高温合金在NaCl熔盐中的循环热腐蚀行为研究
申聚宝, 崔宇, 刘莉, 刘叡, 孟凡帝, 王福会

Cyclic Hot Corrosion Behavior of DZ40M and K452 Superalloys Beneath Molten Deposit NaCl
SHEN Jubao, CUI Yu, LIU Li, LIU Rui, MENG Fandi, WANG Fuhui
图4 DZ40M和K452合金不同周次循环热腐蚀后的表面XRD谱
Fig.4 XRD patterns of DZ40M alloy (a) and K452 alloy (b) after cyclic hot corrosion for different cycles