DZ40M和K452高温合金在NaCl熔盐中的循环热腐蚀行为研究 |
申聚宝, 崔宇, 刘莉, 刘叡, 孟凡帝, 王福会 |
Cyclic Hot Corrosion Behavior of DZ40M and K452 Superalloys Beneath Molten Deposit NaCl |
SHEN Jubao, CUI Yu, LIU Li, LIU Rui, MENG Fandi, WANG Fuhui |
图3 DZ40M和K452合金试样循环热腐蚀不同周次后的宏观形貌 |
Fig.3 Macro morphologies of DZ40M alloy (a-d) and K452 alloy (e-h) after cyclic hot corrosion for 1 cycle (a, e), 2 cycles (b, f), 3 cycles (c, g) and 15 cycles (d, h) |
![]() |