Inconel 718合金在580 ℃下水蒸气环境中的氧化行为及摩擦学性能
贺南开, 王永欣, 周升国, 周大朋, 李金龙

Oxidation Behavior in Water Vapor and Tribological Property in Atmosphere with 60%Relative Humidity at 580 ℃ for Inconel 718 Alloy
HE Nankai, WANG Yongxin, ZHOU Shengguo, ZHOU Dapeng, LI Jinlong
表1 Inconel 718合金在不同载荷下磨痕表面的主要元素
Table 1 Distribution of primary elements on the wear track surface of Inconel 718 alloy under different loads (mass fraction / %)
SpectrumOAlCrFeNiNbMo
19.080.3218.0017.0247.714.902.96
217.280.3816.1216.3743.093.982.78
315.320.4818.4915.2542.015.263.19
422.630.5416.0314.7539.344.022.69