Inconel 718合金在580 ℃下水蒸气环境中的氧化行为及摩擦学性能
贺南开, 王永欣, 周升国, 周大朋, 李金龙

Oxidation Behavior in Water Vapor and Tribological Property in Atmosphere with 60%Relative Humidity at 580 ℃ for Inconel 718 Alloy
HE Nankai, WANG Yongxin, ZHOU Shengguo, ZHOU Dapeng, LI Jinlong
图7 Inconel 718合金在不同载荷下的磨痕、磨斑形貌及磨痕的3D形貌和二维轮廓图
Fig.7 Morphologies of wear tracks (a1-d1) and wear scars (a2-d2), 3D (a3-d3) and 2D (a4-d4) profiles of wear tracks of Inconel 718 alloy at 2 N (a1-a4); 5N (b1-b4); 8N (c1-c4); 10N (d1-d4) loads